摘要 |
PROBLEM TO BE SOLVED: To provide an enclosure for an image display device less in brightness reduction or life shortening, high in display quality, and sufficient in getter effect, by realizing an adhesion process at a temperature about 400 deg.C or below required at the minimum for a frit adhesion (sealing) process. SOLUTION: A rear plate 2 and a face plate 4 are joined respectively at joining parts to an outer frame 3 by an adhesive 9 and sealing material 14. The sealing material is selected from metals or alloys, such as In, Al, Cu, Au, Ag, Pt, Ti, Ni or the like, or organic adhesives, inorganic adhesives or the like with surfaces coated with the metal or the alloy. The adhesive is selected from organic adhesives containing a polyphenyl compound, a polybenzimidazole resin, a polyimide resin or the like, inorganic adhesives containing alumina, silica, zirconia or carbon, or the like.
|