发明名称 |
Activated kaolin powder compound for mixing with cement and method of preparing the same |
摘要 |
The activated kaolin powder compound is prepared from naturally-existing kaolin (hereinafter "natural kaolin"). The activated kaolin powder compound is prepared by heating natural kaolin to 480 DEG C. within at most one hour, calcinating the heated kaolin at high temperature by heating to 980 DEG C. over at least one hour, quenching the calcinated kaolin with water or air, and pulverizing the quenched kaolin to give particle sizes of 2 mu m or less. The activated kaolin powder compound is employed in an amount of about 5 to 15% by weight of cement for preparing mortar or cement. The cement composition containing the activated kaolin powder compound can provide a mortar or concrete having superior properties in compressive strength, flexural strength and water permeability.
|
申请公布号 |
US5976241(A) |
申请公布日期 |
1999.11.02 |
申请号 |
US19970925951 |
申请日期 |
1997.09.08 |
申请人 |
KIM, MOON HAN;KWAK, JEONG HWAN |
发明人 |
KIM, MOON HAN;HWANG, HEY ZOO;HWANG, JUNG HA;CHA, HEE SUNG;KIM, KWANG CHOON;LEE, JONG KUK |
分类号 |
C04B14/10;C04B18/02;C04B22/08;C04B28/02;C04B103/60;C04B111/24;(IPC1-7):C04B14/00 |
主分类号 |
C04B14/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|