摘要 |
<p>PROBLEM TO BE SOLVED: To provide a treating method for plastic, by which plastic can be treated even if films are mixed, and at the same time dehydrochlorination treatment can be performed, and by which plastic processed product which is easily crushed can be obtained, and to provide a solid fuel and a reducing agent for ores each produced by the above treating method. SOLUTION: In the treating method for plastic, after 100 pts.wt. of plastic and 5-40 pts.wt. of coal-based tar and/or distillate of coal-based tar are mixed at 150 deg.C or more to solve and/or swell the plastic, the mixture is cooled and solidified, or is crushed after the cooling and solidifying. A solid fuel and a reducing agent for ores are provided by this treating method.</p> |