摘要 |
<p>The invention relates to tissue products having improved softness properties and methods of making them. Specifically, improved softness is achieved by incorporating a silicone quaternary and, optionally, one or more softeners/debonders into the fiber furnish at the wet end of the tissue machine prior to formation, followed by an optional topical treatment with a silicone quaternary and/or one or more softeners/debonders after the tissue web is formed. The result is a tissue product with added bulk and a smooth surface feel, both properties contributing to improved softness characteristics.</p> |