摘要 |
There is now provided a ceramic material comprising of alumina, 10-50% by volume, preferably 20-35% by volume, silicon carbide whiskers, 1-25% by volume, preferably 5-20% by volume, most preferably 7-15% by volume, zirconia and 1-20% by volume, preferably 3-15% by volume, titanium compound-containing cubic phase. If this cubic phase has a lattice spacing of 4.29 to 4.40 ANGSTROM and a zirconium content of 3-65 weight %, a material with improved performance when turning heat resistant material such as aged Iconel 718, is obtained.
|