This invention relates to a method to manufacture cell-cans by DI can method, by manufacturing a bottomed cylindrical cup-shaped intermediate product from a sheet material of which both surfaces are nickel plated and annealed in an atmosphere of inert gas making the metal nickel layer thickness and the hardness at predetermined values, then ironing the intermediate product at a predetermined ironing rate, securing a thickness of the metal nickel layer of more than 1.0 mu m and a Vickers hardness of more than HV 200 on the side wall of finished cell-cans. By this, conventional defect problems due to the cracks generated on the intermeiate product can be sovled completely and the problem of hair-lines formed on the surface of finished cell-can can be eliminated. <IMAGE>