摘要 |
PCT No. PCT/FR94/01415 Sec. 371 Date Jul. 29, 1996 Sec. 102(e) Date Jul. 29, 1996 PCT Filed Dec. 5, 1994 PCT Pub. No. WO95/16644 PCT Pub. Date Jun. 22, 1995An article comprising a hydrated matrix containing 100 parts by weight of cement and around 80-120 and preferably around 100 parts by weight of sand with a grain size of less than 1 mm, and alkali-resistant reinforcing glass fibres in a proportion of around 3-4 wt %, preferably 3.5 wt %, relative to the hydrated matrix. The article, which has a density no greater than 1.85, may be used as a covering panel for buildings, and particularly as an imitation slate covering panel. |