摘要 |
A modified powder-in-tube process produces a superconductor wire having a significantly greater current density than will a superconductor wire of the same nominal superconductor composition produced using conventional draw-swage-extrude-roll deformation. In the process disclosed, a superconductor precursor is placed within a ductile tube, the tube with the powder therein is then deformed into a cross-section substantially corresponding to that of the end product, and the deformed tube is then subject to a plurality of heat treatments to convert the precursor into the desired superconducting ceramic oxide phase. Before the last of the heat treatments, the tube is isostatically pressed to densify and texture the superconductor precursor oxide in the tube. |