摘要 |
A keiraku-stimulating projection adhesive plaster is prepared by (a) mixing 60-80 parts of Chinese medicines pulverized to 160 mesh, 30-10 parts of PVC powder and 5-15 parts of DOP or DOA; (b) adding 0.1-5 parts of CAB-OSIL; (c) homogenizing it and kneading it with a plasticizer; (d) sticking the Chinese medicines dough (1.5-2.0 mm diameter, 1-3 mm height) on a paper; (e) drying it at room temp. or 150-180 deg.C; and (f) fixing the obtd. projection onto an adhesive plaster.
|