发明名称 Process to reduce roughness of wooden veneer surface - involves hot metal rollers passing over sheet of veneer at least twice in quick succession and then through opposed rotating rollers with different surface roughnesses
摘要 The flat wooden veneer surface is subjected to a defined pressure as a hot metal roller passes over its surface at least twice in quick succession. Sheets of dried veneer are rolled between two opposing rollers rotating at different speeds. The opposing rollers have different degrees of surface roughness. The pressure applied is at least 10<4> N/m, ideally 10<5> N/m and in the direction of wood grain and across the wood grain. Sheets are passed through the rollers in a continual process at a speed of 12 - 20 m/min.The number of pressure cycles is at least as many as the relative speed in M/min between veneer surface and the line of rolling action. The relative speed is 6 -12 m/min. USE/ADVANTAGE - For furniture. Veneers so treated only need a single coat of varnish without any sacrifice in quality. Further, glue, paint and varnish spread uniformly and do not penetrate the veneer when pressure is applied.
申请公布号 DE4213690(A1) 申请公布日期 1993.10.28
申请号 DE19924213690 申请日期 1992.04.25
申请人 BABCOCK-BSH AG VORMALS BUETTNER-SCHILDE-HAAS AG, 4150 KREFELD, DE 发明人 EMMERLING, HANS-JOERG, 7175 VELLBERG, DE;PREHN, KARL, 6430 BAD HERSFELD, DE
分类号 B24B39/06;B27M1/02;F26B7/00;F26B13/18;(IPC1-7):B24B39/06;B30B3/00;F26B15/18 主分类号 B24B39/06
代理机构 代理人
主权项
地址
您可能感兴趣的专利