发明名称 COMPOSITE CHILL CAST IRON ROLLING MILL ROLLS HAVING INCREASED RESISTANCE TO SPALLING
摘要 1,271,185. Rolling. BETHLEHEM STEEL CORP. 23 March, 1970 [24 March, 1969], No. 13893/70. Heading B3M. [Also in Division C7] A composite work roll for cold rolling has a low alloy cast iron core and a chill surface area comprising: the balance, apart from impurities, being Fe. The east rolls may be heated to 850‹ F., held for 4 hours, cooled to 100‹ F. at 50‹ F./hr., reheated to 500‹ F., held for 4 hours, and then cooled to ambient temperature at 50‹ F./hr.; or cooled to - 100‹ F., stress relieved at 500‹ F. at the rate of 1 hour/inch of thickness and then cooled to ambient temperature. The rolls are less susceptible to bruising marking and spalling than prior art rolls. The core of the roll may comprise: the balance, apart from impurities, being Fe.
申请公布号 GB1271185(A) 申请公布日期 1972.04.19
申请号 GB19700013893 申请日期 1970.03.23
申请人 BETHLEHEM STEEL CORPORATION 发明人
分类号 B22D19/16;B21B27/00;C22C37/00 主分类号 B22D19/16