摘要 |
The compsns. (I) comprise (1) 75-99.5 wt.% polymer from (A) 0-95 wt.% graft copolymer obtd. by graft polymerisation of (A1) 5-95 wt.% mixt. of (A1.1) 50-95% styrene, alpha-methylstyrene, nuclearly substd. styrene, and/or Me methacrylate and (A1.2) 50-5 wt.% (meth)acrylonitrile, Me methacrylate,, maleic anhydride, and/or N-substd. maleimide, on, (A2) 95-5 wt.% rubber with max. glass temp. 0 deg.C; (B) 100-5 wt.% thermoplastic polymer from (B1) 95-50 wt.% styrene, alpha-methylstyrene, nuclearly substd. styrene, and/or Me methacrylate and (B2) 5-50 wt.% (meth)acrylonitrile, Me methacrylate, maleic anhydride, and/or N-substd. maleimide; (2) 25-0.5wt.% hydrogenated nitrile rubber.
|
申请人 |
BAYER AG, 5090 LEVERKUSEN, DE |
发明人 |
EICHENAUER, DR., HERBERT, W-4047 DORMAGEN 1, DE;BUDING, DR., HARTMUTH, W-4047 DORMAGEN, DE;DOERING, DR., JOACHIM, W-4018 LANGENFELD, DE;CASPER, PROF. DR., RUDOLF;OTT, DR., KARL-HEINZ, W-5090 LEVERKUSEN 1, DE |