发明名称 |
BORONISING PASTES AND BORONISING TREATMENT METHOD OF FERROUS AND FERROUS-ALLOY SURFACES |
摘要 |
A boronizing agent for iron alloy consists of at least one of 5-60 wt.% B4C, 5-80 wt.% KBF4, 5-40 wt.% SiC and at least 50 wt.% B2O2, and one of accelerating agent and binding agent of at most 30 wt.%. The accelerating agent can be NaCl or Na2CO3 and the binding agent be at least one of alcohol, silicone binder and fluoro binder. A boronizing treatment method of iron and iron alloy surface is characterized by spreading paste of above composition on selected area of substance being boronizing treated and heat-treating it at temperature ranges of 600-1000 deg.C for 1- 10 hrs.
|
申请公布号 |
KR920004014(B1) |
申请公布日期 |
1992.05.22 |
申请号 |
KR19900006469 |
申请日期 |
1990.05.08 |
申请人 |
CHANG, TAE - SUNG;CHON, BYUNG - HO |
发明人 |
CHON, BYUNG - HO |
分类号 |
C23C8/60;(IPC1-7):C23C8/60 |
主分类号 |
C23C8/60 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|