发明名称 |
Method for providing steel with lowered hydrogen level after ladle treatment |
摘要 |
A method is provided for obtaining steel with lowered hydrogen levels after ladle treatment. The method includes covering molten steel in the ladle with a particulate mixture consisting essentially of calcium aluminate and dolomitic limestone. The mixture is used in amounts of about 5 to 25 pounds per net ton of molten steel. Using the method of this invention, some steels to be cast without vacuum degassing to reduce the hydrogen level.
|
申请公布号 |
US5106412(A) |
申请公布日期 |
1992.04.21 |
申请号 |
US19910694615 |
申请日期 |
1991.05.02 |
申请人 |
USX CORPORATION |
发明人 |
BOGAN, ROBERT S.;SESSIONS, KEITH E.;STOLNACKER, DECEASED, WILLIAM J. |
分类号 |
B22D1/00;C21C7/00;C21C7/076 |
主分类号 |
B22D1/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|