摘要 |
This composition, with improved mechanical properties, is based on a mixture of 15-50% by weight of a propylene polymer and of 50-85% by weight of a flexible ethylene copolymer which is a terpolymer (A) containing 83-92.7 mol% of ethylene, 7-14 mol% of alkyl (meth)acrylate and 0.3-3 mol% of unsaturated dicarboxylic acid anhydride; or else a mixture containing, per 100% by weight, at least 70% by weight of terpolymer (A) and not more than 30% by weight of a copolymer (B) chosen from those containing 86-93 mol% of ethylene and 7-14 mol% of alkyl (meth)acrylate, and those containing 88-93 mol% of ethylene and 7-12 mol% of alpha -olefin, with a density of 0.875-0.905, the terpolymer (A) having undergone at an least partial dynamic crosslinking with the aid of a crosslinking agent containing at least one functional group capable of reacting with the anhydride functional group of the said terpolymer (A). |