摘要 |
<P>LA PRESENTE INVENTION A POUR OBJET UN PROCEDE DE PREPARATION D'OXYDE DE LITHIUM DE HAUTE PURETE. SUIVANT L'INVENTION, ON DECOMPOSE DE L'OXYDE DE LITHIUM IMPUR A UNE TEMPERATURE DE 350 A 450 C DANS UNE ATMOSPHERE INERTE ET ANHYDRE POUR PRODUIRE DE L'OXYDE DE LITHIUM IMPUR, ET ON CHAUFFE L'OXYDE DE LITHIUM IMPUR OBTENU SOUS UNE PRESSION QUI N'EST PAS SUPERIEURE A 0,2 KPA A 900 C OU PLUS, PENDANT AU MOINS UNE HEURE POUR OBTENIR DE L'OXYDE DE LITHIUM DE HAUTE PURETE, D'UNE PURETE DE 99 OU PLUS. UN TEL OXYDE DE LITHIUM EST NOTAMMENT UTILE POUR LA PREPARATION DES ACCUMULATEURS AU LITHIUM.</P>
|