发明名称 |
FUNCTIONAL CU-ZN-AL ALLOY |
摘要 |
<p>PURPOSE:To obtain a functional Cu-Zn-Al alloy with especially stabilized temp. sensitivity and enhanced resistance to thermal fatigue due to repeated use, by adding a specified precentage of Fe and/or P to a Cu-Zn-Al alloy and by alloying them. CONSTITUTION:0.01-1.0% Fe, 0.01-0.05% P and/or 0.01-0.1% B are added to a Cu-Zn-Al alloy consisting of 68-72% Cu, 2.8-4.5% Al and the balance Zn to obtain a functional Cu-Zn-Al alloy. This alloy is a shape memory alloy contg. martensite having <=500mum, especially <=100mum average grain size. This shape memory alloy has remarkably improved temp. sensitivity, shape restoring power and fatigue resistance. Unsatisfactory shape restoring power and fatigue resistance are considered to be the maximum defects of a convertional alloy.</p> |
申请公布号 |
JPS58171542(A) |
申请公布日期 |
1983.10.08 |
申请号 |
JP19820053441 |
申请日期 |
1982.03.31 |
申请人 |
DOUWA KOGYO KK;NIHON BURASU KOGYO KK;DOUWA KINZOKU KOGYO KK |
发明人 |
OOYAMA SHIGERU;KAI HIROYUKI;ASANO TOSHIO;KASASHIMA TAKEFUMI;ASAKURA TAKESHI;KUROSAWA TOSHIO;KATOU TADAAKI |
分类号 |
C22C9/00;C22C9/04;C22F1/00;C22F1/08 |
主分类号 |
C22C9/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|