发明名称 COPPER LEACHING PROCESS EMPLOYING NITROGEN DIOXIDE
摘要 <p>K-0508-KCC Sulfidic minerals containing metal values such as copper, silver, nickel, cobalt, molybdenum, zinc, iron, or mixtures thereof are oxidized with nitrogen dioxide to enable the metal values to be solubilized in an aqueous acidic leach liquor. In practicing the invention, the minerals are added to an aqueous acidic leach liquor and a nitrogen dioxide containing gas is sparged through the slurry to oxidize the metal values. During the reaction, the nitrogen dioxide is reduced to nitric oxide. The nitric oxide is oxidized to nitrogen dioxide by oxygen, either in situ, or in a separate off-gas oxidizer.</p>
申请公布号 CA1110077(A) 申请公布日期 1981.10.06
申请号 CA19780308749 申请日期 1978.08.04
申请人 KENNECOTT COPPER CORPORATION 发明人 FRANKIEWICZ, THEODORE C.;LUEDERS, ROBERT E.
分类号 C22B3/06;C22B15/00;(IPC1-7):22B15/08 主分类号 C22B3/06
代理机构 代理人
主权项
地址