摘要 |
<p>The durability of coatings formed from antifouling compositions containing a biologically active organotin-containing polymer as the film-forming component is improved by the presence of at least one organotin-containing polymer which is not necessarily biologically active in an amount of from 0.01 to 10% based on the weight of the initial coating composition. In the biologically active polymer, at least 25 mole % of the repeating units contain a triorganotin moiety, whereas in the other polymer not more than 15 mole % of the repeating units contain tin.</p> |