发明名称 |
Elastic terpolymer and preparation method thereof |
摘要 |
The present invention relates to an elastic terpolymer that can acquire good mechanical properties and elasticity (flexibility) at the same time, and a preparation method thereof.;The elastic terpolymer, which is a copolymer of 40 to 70 wt % of ethylene, 15 to 55 wt % of a C3-C20 alpha-olefin, and 0.5 to 20 wt % of a diene as obtained in the presence of a group 4 transition metal catalyst, satisfies that: (i) the weight average molecular weight measured by GPC is 100,000 to 500,000; and (ii) the ethylene content x (wt %) and the crystallization enthalpy y (ΔHcJ/g) of the copolymer measured by DSC satisfy a defined relational expression. |
申请公布号 |
US9458276(B2) |
申请公布日期 |
2016.10.04 |
申请号 |
US201214440563 |
申请日期 |
2012.11.15 |
申请人 |
LG Chem, Ltd. |
发明人 |
Yoon Sung-Cheol;Ko Jun-Seok;Park Sung-Ho;Choi Soo-Young |
分类号 |
C08F210/18;C08F236/20;C08F4/659 |
主分类号 |
C08F210/18 |
代理机构 |
Dentons US LLP |
代理人 |
Dentons US LLP |
主权项 |
1. An elastic terpolymer, which is a copolymer of 40 to 70 wt % of ethylene, 15 to 55 wt % of a C3-C20 alpha-olefin, and 0.5 to 20 wt % of a diene as obtained in the presence of a group 4 transition metal catalyst, wherein the elastic terpolymer satisfies that:
the weight average molecular weight measured by GPC is 100,000 to 500,000; and ii) the ethylene content x (wt %) and the crystallization enthalpy y (ΔHc; J/g) of the copolymer measured by DSC satisfy the relational expression given by 1.55x−80.00≦y≦1.55x−75.00. |
地址 |
Seoul KR |