发明名称 可鍛鋳鉄の熱処理方法および鋳物の製造方法
摘要 PROBLEM TO BE SOLVED: To provide a heat treatment method for malleable cast iron capable of obtaining a casting having excellent plating properties.SOLUTION: This method is one treatment for producing a casting obtained by generating a plating layer on the surface of a casting stock made of malleable cast iron, and, in heat treatment for malleable cast iron after the casting of the casting stock, using a vessel for heat treatment having a loading chamber made air-tight to the ambient air and having a vessel for heat treatment heated in a heating furnace. The casting stock is loaded into the loading chamber of the vessel for heat treatment and is annealed, and is thereafter subjected to a cooling step of being cooled at a cooling rate of 100 to 5,000°C/h till the casting stock reaches 575°C or lower.
申请公布号 JP6019850(B2) 申请公布日期 2016.11.02
申请号 JP20120156450 申请日期 2012.07.12
申请人 日立金属株式会社 发明人 後藤 亮
分类号 C21D5/06;C23C2/02 主分类号 C21D5/06
代理机构 代理人
主权项
地址