发明名称 タンデムガスシールドアーク溶接方法
摘要 A torch angle ¸ L of a leading electrode that uses a solid wire and a torch angle ¸ T of a trailing electrode that uses a flux-cored wire are respectively set in the following ranges: 5° ‰¤ ¸ L < 40° and 40° ‰¤ ¸ T ‰¤ 60°. A 100% carbon dioxide gas is used as a shielding gas for both the electrodes. In this state, a welding voltage V L and a welding current I L , which are welding parameters of the leading electrode, are respectively 26 to 38 V and 350 to 550 A, and the welding voltage V L in V and the welding current I L in A satisfy the following relationship: 56 ‰¤ (V L ·10 3 /I L ) ‰¤ 84.
申请公布号 JP6025627(B2) 申请公布日期 2016.11.16
申请号 JP20130057326 申请日期 2013.03.19
申请人 株式会社神戸製鋼所 发明人 袁 倚旻;山崎 圭;鈴木 励一