Ferrous alloy for coining and method for producing the same |
摘要 |
A ferrous alloy is provided for coining The ferrous alloy includes a composition of: 4.00-10.80 wt % of chromium (Cr), 8.00-25.00 wt % of nickel (Ni), 3.00-6.00 wt % of copper (Cu), and a balance of iron (Fe) and incidental impurities. |
申请公布号 |
US9351547(B2) |
申请公布日期 |
2016.05.31 |
申请号 |
US201313793183 |
申请日期 |
2013.03.11 |
申请人 |
CRS Holdings Inc. |
发明人 |
Pilliod Christopher F. |
分类号 |
C22C38/42;C21D8/00;C21D7/00;A44C21/00;C22C1/02;C22C38/58;C22C38/34;B21B1/02;B21D19/00;B21D28/02;B24B1/00;C21D6/00;C22C38/02;C22C38/04 |
主分类号 |
C22C38/42 |
代理机构 |
Barley Snyder |
代理人 |
Barley Snyder |
主权项 |
1. A ferrous alloy for coining, consisting essentially of:
4.00-9.85 wt % of chromium (Cr); 8.00-25.00 wt % of nickel (Ni); 3.00-6.00 wt % of copper (Cu); 0.001-0.025 wt % of C; 0.50-2.00 wt % of Mn; 0.001-2 wt % of Si; and a balance of iron (Fe) and incidental impurities. |