发明名称 METHOD OF MAKING SULFUR EXTENDED ASPHALT MODIFIED WITH CRUMB RUBBER
摘要 The present invention relates to asphalt compositions. The present invention provides for a sulfur rubber asphalt binder composition that includes a base asphalt having a softening point, elemental sulfur, and a crumb rubber material. The crumb rubber material is combined with the base asphalt and the elemental sulfur to create the sulfur rubber asphalt binder composition. The crumb rubber material is present in the sulfur rubber asphalt binder in an amount effective to increase the softening point as compared to the softening point of the base asphalt.
申请公布号 US2016108242(A1) 申请公布日期 2016.04.21
申请号 US201514874030 申请日期 2015.10.02
申请人 Saudi Arabian Oil Company ;King Fahd University of Petroleum and Minerals 发明人 Al-Mehthel Mohammed;Parvez Mohammad Anwar;Al-Abdul Wahhab Hamad I.;Hussein Ibnelwaleed A.;Al-Idi Saleh H.
分类号 C08L95/00;C08L21/00 主分类号 C08L95/00
代理机构 代理人
主权项 1. A method of making a sulfur rubber asphalt binder composition comprising the steps of: mixing the crumb rubber material with the base asphalt at a first predetermined temperature in a high shear blender for first predetermined amount of time to create an asphalt crumb rubber mixture; placing the asphalt crumb rubber mixture in a sealed container in an oven at the first predetermined temperature for a second predetermined amount of time; adding elemental sulfur to the asphalt crumb rubber mixture and mixing for a third predetermined amount of time at a second predetermined temperature such that intimate mixing of the elemental sulfur and the asphalt crumb mixture is achieved.
地址 Dhahran SA