发明名称 |
METHOD FOR PRODUCING PIG IRON AND BLAST FURNACE FACILITY USING SAME |
摘要 |
This blast furnace facility is provided with: a blast furnace main body (110); starting material charging means (111,113) that charge a starting material (1) containing iron ore and coke into the interior of the blast furnace main body (110) from the apex thereof; hot airflow blow in means (114, 115) that blows in a hot airflow (101) from a tuyere to the interior of the blast furnace main body (110); and blast furnace blow in charcoal supply means (120, 129) that blow in blast furnace blow in charcoal (11) from the tuyere to the interior of the blast furnace main body (110). The blast furnace blow in charcoal supply means (120, 129) blow in a blast furnace blow in charcoal (11) having an oxygen atom content (on a dry basis) of 10 20 wt% and an average pore size of 10 50 nm. |
申请公布号 |
IN11082DEN2014(A) |
申请公布日期 |
2015.09.25 |
申请号 |
IN2014DELNP11082 |
申请日期 |
2014.12.24 |
申请人 |
MITSUBISHI HEAVY INDUSTRIES LTD. |
发明人 |
OMOTO SETSUO;NAKAGAWA KEIICHI;HAMADA TSUTOMU;SAKAGUCHI MASAKAZU |
分类号 |
C21B5/00;C10B53/00;C10B57/10 |
主分类号 |
C21B5/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|