发明名称 METHOD FOR MANUFACTURING LITHIUM ALUMINATE HAVING SLENDER PARTICLE SHAPE
摘要 PROBLEM TO BE SOLVED: To provide lithium aluminate having a slender particle shape useful for electrolyte holding plate applications of a molten carbonate fuel cell (MCFC) by an industrially useful method.SOLUTION: There is provided a method for manufacturing lithium aluminate having a slender particle shape including a reaction process of heating and reacting raw material mixture solution containing lithium hydroxide, an aluminum source, alkali hydroxide represented by MOH, where M represents Na or K, and an aqueous solvent with a molar ratio of M/Al of 2 or more and a molar ratio of Li/Al of 1.7 or more.