摘要 |
The present invention is directed to metallurgical powder compositions having improved lubricant properties. These compositions of the invention include at least 90 wt.% of an iron based metallurgical powder; a Group 1 or Group 2 metal stearate; a first wax having a melting range of between about 80 and 100 °C; a second wax having a melting range of between about 80 and 90 °C; inc phosphate; boric acid; acetic acid; phosphoric acid; and polyvinylpyrrolidone. Methods of compacting the compositions as well as compacted articles prepared using those methods are also described. |