发明名称 |
Bituminous paving composition and process for bituminous paving |
摘要 |
The invention provides a bituminous composition, a process for preparing a bituminous paving composition and process for bituminous paving having lower mixing, paving, and compaction temperatures than for conventional hot-mix paving while retaining sufficient performance characteristics of conventional hot-mix paving. The inventive paving process comprises the steps of injecting a foamable solution comprising a lubricating substance into a heated, asphalt binder to provide a heated, foamed mixture; adding the heated, foamed mixture to a suitable, heated aggregate; further mixing the heated, foamed mixture and heated aggregate to coat the heated aggregate with the heated, foamed, asphalt binder to form a heated paving material; supplying the heated paving material to a paving machine; applying the heated paving material by the paving machine to a surface to be paved; and compacting the applied paving material to form a paved surface. |
申请公布号 |
US8828135(B2) |
申请公布日期 |
2014.09.09 |
申请号 |
US201313907108 |
申请日期 |
2013.05.31 |
申请人 |
ALM Holding Company |
发明人 |
Reinke Gerald H. |
分类号 |
C08L95/00;E01C7/18;E01C7/26;B28C5/00;E01C19/22 |
主分类号 |
C08L95/00 |
代理机构 |
Kagan Binder, PLLC |
代理人 |
Kagan Binder, PLLC |
主权项 |
1. A process of preparing a warm mix paving composition comprising the steps of:
a) combining an aqueous solution, the aqueous solution comprising water and a lubricating substance, with an asphalt binder heated to a warm mix temperature of about 230-325° F. to provide a heated foamed asphalt binder, and b) mixing the heated foamed asphalt binder with aggregate heated to a temperature of about 180-300° F. to coat the aggregate and form a warm mix paving composition containing asphalt binder, lubricating substance and aggregate, wherein the process reduces the thermal energy used to achieve suitable mixing and paving compared to a conventional hot mix paving composition prepared from the asphalt binder without the aqueous solution, and without adversely affecting paving using the warm mix paving composition. |
地址 |
Onalaska WI US |