发明名称 Improvenment material of early age strength using industrial by products
摘要 The present invention relates to environmentally-friendly mortar and concrete compositions which can have high compression strength with a small amount of cement and use industrial byproducts as a main component. The compositions are prepared by mixing 100 parts by weight of combustible calcium hydroxide, 20-40 parts by weight of II-type of anhydrous gypsum, 20-40 parts by weight of alumina, and 40-60 parts by weight of furnace slag powder.
申请公布号 KR101394783(B1) 申请公布日期 2014.05.15
申请号 KR20120071163 申请日期 2012.06.29
申请人 发明人
分类号 C04B18/06;C04B18/14;C04B28/16 主分类号 C04B18/06