摘要 |
A method for producing a polarizer (20) comprises the steps of: (A) stretching a polyvinyl alcohol-based resin layer (10) to obtain a stretched layer (14); (B) immersing the stretched layer (14) in a dyeing liquid (23) containing iodine to obtain a dyed layer (18) in which absorbance thereof determined from a tristimulus value Y is from 0.4 to 1.0 (transmittance T = 40% to 10%); and (C) removing a part of iodine adsorbed in the dyed layer (18) so that the absorbance of the dyed layer (18) decreases by 0.03 to 0.7, provided that the absorbance of the dyed layer (18) is controlled so that it does not become less than 0.3. |