摘要 |
A method is indicated for producing a lithium titanium mixed oxide, comprising the provision of a mixture of titanium dioxide and a lithium compound, calcining of the mixture, and grinding of the mixture in an atmosphere with a dew point <-50° C. A lithium titanium mixed oxide and a use of same are also indicated. In addition, an anode and a solid electrolyte for a secondary lithium-ion battery, as well as a corresponding secondary lithium-ion battery are provided. |