摘要 |
A halogen free flame-retardant polymer composition includes flame retardancy and excellent oil resistance/fuel resistance, low-temperature characteristics, and injury resistance, and an insulated electric wire and a cable include the composition. The halogen-free flame-retardant polymer composition includes a base polymer including 60 to 70% by mass of LLDPE, 10% by mass or more of EVA having a melt flow rate (MFR) of 100 or more, and 10 to 20% by mass of maleic acid-modified polyolefin, a metal hydroxide added at a ratio of 150 to 220 parts by mass relative to 100 parts by mass of the base polymer, and carbon black. The addition ratio (metal hydroxide/carbon black) between the metal hydroxide and the carbon black is 15:1 to 100:1. |