摘要 PROBLEM TO BE SOLVED: To provide an Ni-based heat-resistant alloy excellent in creep strength and creep ductility after being used at high temperature for a long time.SOLUTION: An Ni-based heat-resistant alloy contains, by mass, 0.1% or less C, 1% or less Si, 1% or less Mn, 15.0% to below 28.0% Cr, 3-18% of Mo+0.5W, 0.5% to 2.5% Al, over 0.5% to 2.0% Ti, 0.1-2.0% Nb, and 0.0005-0.01% B, with the balance comprising 50% or more Ni and impurities, and satisfies formula (1) and formula (2), with the proviso that the strain in lattice matching between the precipitated phase and the matrix phase is 0.4% or less, and the volume fraction of a gammer prime phase at 750°C is 25 mol% or less, wherein formula (1): Al-Ti≥-0.1 and formula (2): Al-(Ti+Nb) ≤0.1 are satisfied. In formulae (1) and (2), the element symbols are substituted by the contents (mass%) of the corresponding elements.
申请公布号 JP2013216939(A) 申请公布日期 2013.10.24
申请号 JP20120087868 申请日期 2012.04.06
申请人 NIPPON STEEL & SUMITOMO METAL CORP 发明人 YONEMURA MITSUHARU;SENBA MITSUYUKI;HAMAGUCHI TOMOAKI;IGARASHI MASAAKI
分类号 C22C19/05 主分类号 C22C19/05
代理机构 代理人
主权项
地址
您可能感兴趣的专利