发明名称 TEMPERED GLASS AND TEMPERED GLASS SHEET
摘要 Provided is a tempered glass having a compression stress layer in a surface thereof, comprising, as a glass composition in terms of mol %, 50 to 75% of SiO2, 3 to 13% of Al2O3, 0 to 1.5% of B2O3, 0 to 4% of Li2O, 7 to 20% of Na2O, 0 to 10% of K2O, 0.5 to 13% of MgO, 0 to 6% of CaO, and 0 to 4.5% of SrO, and being substantially free of As2O3, Sb2O3, PbO, and F.
申请公布号 US2013017380(A1) 申请公布日期 2013.01.17
申请号 US201213569633 申请日期 2012.08.08
申请人 MURATA TAKASHI;TOJYO TAKAKO;KAWAMOTO KOSUKE;TOMITA YUUSUKE 发明人 MURATA TAKASHI;TOJYO TAKAKO;KAWAMOTO KOSUKE;TOMITA YUUSUKE
分类号 B32B17/06;B32B7/02;C03C3/085;C03C3/087;C03C3/091;C03C21/00 主分类号 B32B17/06