发明名称
摘要 <p>Production of an adhesive layer containing at least one isocyanate reactive polymer and a solid surface-deactivated polyisocyanate and to increase its shear strength, comprises heat treatment at a temperature, preferably &ge; 40 degrees C above the drying temperature. The shear strength of the resulting adhesive joint is at least 10% higher than without the heat treatment. A process for the production of an adhesive layer and to increase its shear strength comprises: (A) preparation of an aqueous dispersion or solution containing at least one isocyanate reactive polymer and a solid surface-deactivated polyisocyanate; (B) application of the aqueous dispersion or solution onto a substrate; (C) production of an adhesive layer by removal of the water by drying at 20-95 degrees C (preferably 50-95 degrees C); and (D) performing heat treatment where the layer is heated continuously, stepwise or directly to a temperature, preferably at least 40 degrees C above the drying temperature. The shear strength of the resulting adhesive joint is at least 10% higher than without the heat treatment and the isocyanate reactive polymer and the solid surface-deactivated polyisocyanate are chosen such that following step (C), the adhesive layer has a loop tack of at least 2 N/inch.</p>
申请公布号 JP5081362(B2) 申请公布日期 2012.11.28
申请号 JP20020510571 申请日期 2001.05.21
申请人 发明人
分类号 C09J5/00;C09J7/02;C08G18/50;C08G18/62;C08G18/70;C09J175/04 主分类号 C09J5/00
代理机构 代理人
主权项
地址