Method for restoring antimicrobial hydrophilic coatings
摘要
<p>A method for restoring a silver oxide-containing hydrophilic coating includes heating the coating to a temperature between about 260 °C and about 540 °C and maintaining the coating at a temperature between about 260 °C and about 540 °C in an environment containing oxygen and ozone for less than 24 hours.</p>
申请公布号
EP2505617(A1)
申请公布日期
2012.10.03
申请号
EP20120160311
申请日期
2012.03.20
申请人
HAMILTON SUNDSTRAND SPACE SYSTEMS INTERNATIONAL, INC.