摘要 <p>An improved method for processing of nickel laterite ores to recover the valuable minerals contained therein, comprising comminuting ore to a desired size; leaching the ore at about 70C to 130C for about 30 minutes to 4 hours with nitric acid, raising the temperature of the solution to form a liquid/solid residue in which nickel, cobalt and magnesium values are in solution, and iron, manganese, and aluminum are solid residues in oxide form; conducting a liquid-solid separation and removing the solids; and recovering the nickel, cobalt, and manganese from the liquid-metal concentrate. The leachate is recovered and the nitric acid from the leachate is recycled.</p>