摘要 |
A glass substrate of the present invention for magnetic recording media having high heat resistance and easy chemical strengthening ability at once has not been obtained, which is a glass composition essentially comprising 60 to 70 wt % SiO2, 5 to 20 wt % Al2O3, 0 to 1 wt % Li2O, 3 to 18 wt % Na2O, 0 to 9 wt % K2O, 0 to 10 wt % MgO, 1 to 15 wt % CaO, 0 to 4.5 wt % SrO, 0 to 1 wt % BaO, 0 to 1 wt % TiO2 and 0 to 1 wt % ZrO2, wherein the sum of Li2O, Na2O and K2O is from 5 to 25 wt %, and the sum of MgO, CaO, SrO and BaO is from 5 to 20 wt %.
|