摘要 |
An oil-repellent coating layer 2 is disposed on both surfaces of a lens material 1 consisting of glass or a plastic. Furthermore, a minute particle layer 3 in which minute particles of a metal oxide or minute particles of a fluoride, or both, are dispersed is formed on the surface of the oil-repellent coating layer 2, and a resin layer 4 consisting of an organic compound is disposed on the surface of the minute particle layer 3. Since the adhesion between the resin layer 4 and the two-sided adhesive tape that is used when the lens is set in the lens edging machine is good, axial shifting tends not to occur during working. |