PROBLEM TO BE SOLVED: To precisely form a stereoscopically swelled coating layer by adopting an inkjet coating method at a part of a coating step using a reaction curing type coating material. SOLUTION: The coating method is carried out by applying a coating material base compound 1 on a base material 2, jetting a curing agent 3 for the coating material base compound 1 on the coating material base compound 1 applied on the base material 2 to form an optical pattern and curing the coating material base component 1 applied on the base material 2 only on an optional pattern part where the curing agent 3 is applied. And then the curing agent for the coating material base compound 1 applied on the base material 2 and a non reacted part are removed. COPYRIGHT: (C)2008,JPO&INPIT
|