摘要 |
PROBLEM TO BE SOLVED: To provide a flame-retardant profile extrusion resin product having mechanical characteristics, transparency, weather resistance, electrical and thermal characteristics essential to an aromatic polycarbonate resin and suppressed bleedout of a flame retardant during extrusion. SOLUTION: The flame-retardant profile extrusion resin product is obtained by extruding a resin composition containing (B) a perfluoroalkylsulfonate in an amount of 0.01-0.5 pt.wt. based on (A) 100 pts.wt. of an amorphous resin having≥15 MVR-R (melt volume flow rate ratio) represented by general formula (1) MVR-R=MVR<SB>21.6</SB>/MVR<SB>2.16</SB>(1) (wherein, MVR<SB>2.16</SB>represents the MVR measured at 280°C under 2.16 kg load according to JIS K 7210; and MVR<SB>21.6</SB>represents the MVR measured at 280°C under 21.6 kg load according to JIS K 7210). COPYRIGHT: (C)2007,JPO&INPIT
|