发明名称 |
Method for preparing styrenic resin having high impact strength and gloss |
摘要 |
The present invention relates to a preparation method for acrylonitrile-butadiene-styrene resin by continuous bulk polymerization comprising the following steps of a) preparing a mixed solution of styrene monomers and acrylonitrile monomers by adding 5-10 weight % of the mixture of styrene monomers and acrylonitrile monomers to a reaction solvent; b) preparing a polymerization solution by dissolving butadiene rubber in the above mixed solution of styrene monomers and acrylonitrile monomers; c) polymerizing with a serial injection of the prepared polymerization solution and initiator in a grafting reactor; d) polymerizing the reaction solution of the above c) in a phase inversion reactor by adding 90-95 weight % of the total mixture of styrene monomers and acrylonitrile monomers thereto; and e) polymerizing further the reaction solution of the above step d) at 130-160° C. The resin prepared by the method of the present invention thus has excellent impact strength and gloss.
|
申请公布号 |
US7132474(B2) |
申请公布日期 |
2006.11.07 |
申请号 |
US20050222164 |
申请日期 |
2005.09.08 |
申请人 |
LG CHEM. LTD. |
发明人 |
SEO JAE-BURN;KIM SANG-SEOP;HAN CHANG-HUN |
分类号 |
C08F297/04 |
主分类号 |
C08F297/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|