发明名称 |
Wärmeschrumpfbarer Polyesterfilm |
摘要 |
In a thermo-shrinkable polyester film, the thermal shrinkage ratio in a main shrinking direction is about 20% or more after being treated in water of about 70 DEG C for about 5 seconds, about 35 to about 55% after treated in water of about 75 DEG C for about 5 seconds, and about 50 to about 60% after being treated in water of about 80 DEG C for about 5 seconds. After the film is shrunk by about 5% by treatment in water of about 75 DEG C for about 10 seconds, the probability of the elongation at rupture of the film in the direction perpendicular to the main shrinking direction being about 20% or less, is about 10% or less. |
申请公布号 |
DE69924421(T2) |
申请公布日期 |
2006.03.09 |
申请号 |
DE1999624421T |
申请日期 |
1999.01.29 |
申请人 |
TOYO BOSEKI K.K., OSAKA |
发明人 |
MORI, KUNIHARU;INOUE, MITSUO;OKUMURA, SHINICHIRO;OKO, TSUTOMU;TABOTA, NORIMI;HASHIMOTO, MASATOSHI;ITO, HIDEKI;TAKABAYASHI, SEIZO;ISAKA, TSUTOMU |
分类号 |
B29C61/00;B29C61/06;B29C63/42;C08J5/18 |
主分类号 |
B29C61/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|