发明名称 METHOD FOR CRUSHING/SHREDDING WOODEN BIOMASS AND GASFICATION METHOD
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a method for improving a crashing property of wooden biomass raw material by specifying the ranges of heating temperature and heating time, and to provide a method for improving the crushing property and the opening property of bamboo. <P>SOLUTION: In the methods for crushing/shredding the wooden biomass, the wooden biomass raw material is thermally degraded at the temperature of≥240°C to≤300°C for the time of≥15 min to≤90 min, thereafter, is crushed and, as a result, the crushing property is improved while suppressing pulverization. Further, in this method, the bamboo is thermally degraded at the temperature of≥170°C to≤220°C for the time of≥15 min to≤120 min, thereafter, is crushed and, as a result, the strength between fibers is weakened while maintaining the strength in a fiber direction. <P>COPYRIGHT: (C)2006,JPO&NCIPI</p>
申请公布号 JP2006026474(A) 申请公布日期 2006.02.02
申请号 JP20040205760 申请日期 2004.07.13
申请人 NIPPON STEEL CORP 发明人 HASHIMOTO SHIGERU;KAWAMURA TAKAFUMI;NAKAMURA MASAKAZU
分类号 B02C19/18;B09B3/00;C10B53/02;C10J3/00 主分类号 B02C19/18
代理机构 代理人
主权项
地址