摘要 |
An explosive composition is provided that includes 85 to about 96 weight percent nitramine based on the total composition weight, and about 4 to 15 weight percent plasticized binder. At least 80 weight percent of the total composition weight, and more preferably 85 to 96 weight percent of the total composition weight, comprises 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazatetracyclo[5.5.0.05,903,11]-dodecane (CL-20) particles having an average particle size not greater than 30 microns as the nitramine. Methods for preparing an explosive from the explosive composition are also provided.
|