摘要 |
PROBLEM TO BE SOLVED: To provide a release film for obtaining a ceramic green sheet having a good dimensional shape (particularly at a lateral end) without bringing about a repellance in the case of coating a ceramic paint on a release layer, by optimizing release layer coating conditions after the paint is resultantly released from the release film. SOLUTION: The release film comprises the release layer 2 provided on at least one surface of a base film 1. The release film further comprises the uncoating parts 5 of the layer 2 at both lateral ends of the base film 1, in such a manner that, when an oil base ink 9 is coated so as to include the end 4 and the uncoating part 5 of the layer 2, the repelling part 8 of the ink 9 has a length of 2.0 mm in the lateral direction from the end 4 to the uncoating part 5.
|