发明名称 PRODUCTION METHOD FOR CORROSION-RESISTANT, HIGH-STRENGTH OIL WELL STEEL PIPE JOINT AND HIGH-STRENGTH OIL WELL STEEL PIPE JOINT
摘要 PROBLEM TO BE SOLVED: To provide a production method by welding of a high-strength oil well steel pipe joint. SOLUTION: The production method includes a high-strength martensitic stainless steel pipe, base metal of which is composed in mass of C of 0.03% or less, Si of 0.70% or less, Mn of 0.30-2.00%, Cr of 10.5-15.0%, Ni of 0.03% or less, O of 0.01% or less and either one or both of Nb of 0.20% or less and/or V of 0.20% or less. The production method further includes a welding filler metal composed in mass of C+N of 0.3% or less, Si of 1.0% or less, Mn of 2.5% or less, Cr of 10.5-24.0%, Ni of 8.0% or less and either one or both of Nb of 0.20% or less and/or V of 0.20% or less. The circumferential edges of the said pipes are welded together by filling the sail filler metal to form a pipe joint. Or welding conditions or the base metal is adjusted so that the filler metal can further contain Mo, Cu, Ti, Zr, B, W, Ca and REM. The base metal can further contain Mo, Cu, Ti, Zr, B, W and Ca.
申请公布号 JP2002137058(A) 申请公布日期 2002.05.14
申请号 JP20000326699 申请日期 2000.10.26
申请人 KAWASAKI STEEL CORP 发明人 KIMURA MITSUO;MIYATA YUKIO;TOYOOKA TAKAAKI
分类号 F16L13/02;B23K9/028;B23K9/23;B23K101/06;C22C38/00;C22C38/58;F16L9/02;(IPC1-7):B23K9/028 主分类号 F16L13/02
代理机构 代理人
主权项
地址