发明名称 |
MAGNETIC DISK COMPRISING FIRST CARBON COATING FILM HAVING HIGH SP3 CONTENT AND SECOND CARBON COATING FILM HAVING LOW SP3 CONTENT |
摘要 |
PROBLEM TO BE SOLVED: To provide a method for forming an improved carbon protective coating film without affecting large influence on a antifliction system between a disk and a head in a magnetic disk having the carbon protective coating film and to provide a magnetic disk having the improved carbon protective coating film. SOLUTION: The method for manufacturing the magnetic disk comprises the formation of a first and a second protective carbon layer on the magnetic disk. The first protective carbon layer comprises SP3 dominant carbon. The second protective carbon layer comprises 50% or less SP3 carbon. The second protective carbon layer has very thin thickness, e.g. 0.1-1.0 nm thickness. A lubricating layer (e.g. perfluoropolyether lubricant) is applied onto the second protective carbon layer. The second protective carbon layer promotes improved cooperation between the disk and the lubricant. |
申请公布号 |
JP2002063717(A) |
申请公布日期 |
2002.02.28 |
申请号 |
JP20010192251 |
申请日期 |
2001.06.26 |
申请人 |
KOMAG INC |
发明人 |
LAIRSON BRUCE;TSOI CHING JACKIE;LIU WEN;HASHIMOTO SHIGETO;YONG ERIC WOO HOCK;YAMASHITA TSUTOMU TOM |
分类号 |
C23C14/34;C23C14/06;C23C16/26;G11B5/72;G11B5/84;G11B5/85;G11B5/851;(IPC1-7):G11B5/84 |
主分类号 |
C23C14/34 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|