摘要 |
A multi-layer antireflection coating is formed to include successive layers of a medium refractive index material, a high refractive index material, and a low refractive index material. The medium refractive index layer is hydrogenated in order to tailor the refractive index of the material to below 1.99 and to increase clarity in transmission. Preferably, the hydrogen atomic concentration is at least 7 percent, more preferably exceeds 9 percent, and most preferably exceeds 18 percent. The three layers combine to form a three-layer antireflection coating, but the hydrogenation may be used in antireflection coatings having a greater or lesser number of layers. |