发明名称 |
CELL AND METHOD OF PRODUCING THE SAME |
摘要 |
<p>In a conventional battery containing metal lithium in the negative electrode, there is a problem that large short-circuit current was generated with temperature rise due to internal short-circuit or the like, and therefore, the temperature of the battery further increases due to exothermic reaction to increase the short-circuit current. The present invention has been carried out in order to solve the above problems. The battery of the present invention comprises a negative electrode 2 containing lithium metal, a positive electrode 1 containing a positive electrode active material 8 and an electronically conductive material 9 contacted to the positive electrode active material 8, and an electrolytic layer 3 between the positive electrode 1 and the negative electrode 2, wherein the electronically conductive material 9 comprises an electrically conductive filler and a resin and resistance thereof is increased with temperature rise. <IMAGE></p> |
申请公布号 |
EP1104037(A1) |
申请公布日期 |
2001.05.30 |
申请号 |
EP19980929698 |
申请日期 |
1998.06.25 |
申请人 |
MITSUBISHI DENKI KABUSHIKI KAISHA |
发明人 |
YOSHIOKA, SHOJI;KISE, MAKIKO;URUSHIBATA, HIROAKI;SHIOTA, HISASHI;ARAGANE, JUN;AIHARA, SHIGERU;TAKEMURA, DAIGO;NISHIMURA, TAKASHI |
分类号 |
H01M4/62;H01M10/05;H01M10/42;(IPC1-7):H01M4/62;H01M2/34;H01M4/02;H01M10/40 |
主分类号 |
H01M4/62 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|